Polymer Property : Tensile Strength at Break = 174000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 900 - 1200 MPa
131000 - 174000 psi
Longitudinal
Goodfellow Carbon/Vinyl Ester Rod
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Tensile Strength at Break 900 - 1200 MPa
131000 - 174000 psi
Longitudinal
Goodfellow Carbon/Vinyl Ester Tube
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Tensile Strength at Break 480 - 1200 MPa
69600 - 174000 psi
Goodfellow Nickel 70/Copper 30 Alloy
Information provided by Goodfellow.