Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.8 - 17.2 MPa | 2000 - 2500 psi | |
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 13.8 - 17.2 MPa | 2000 - 2500 psi | |
ITW Plexus Plexusâ„¢ MA320 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent low temperature and toughness properties.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 13.8 - 17.2 MPa | 2000 - 2500 psi | |
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 13.8 - 17.2 MPa | 2000 - 2500 psi | |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 13.8 - 17.2 MPa | 2000 - 2500 psi | |
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 13.8 - 17.2 MPa | 2000 - 2500 psi | |
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g.. |