Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.62 - 10.3 MPa | 1250 - 1500 psi | |
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works. |