Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.797 MPa | 1421 psi | ASTM D412 |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Tensile Strength at Break | >= 9.797 MPa | >= 1421 psi | ZCI-T-008 |