Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.3 MPa | 2070 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible MG26 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 14.3 MPa | 2070 psi | IEC 60811 |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Tensile Strength at Break | 14.3 MPa | 2080 psi | ASTM D638 |
LyondellBasell Alathon® M4621 High Density Polyethylene ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste.. |
|||
Tensile Strength at Break | 14.3 MPa | 2070 psi | ISO R 527 |
Stir SpA CT 65 ATC (PVC) Application: Tread, pure plasticInformation provided by STIR SpA |
|||
Tensile Strength at Break | 14.3 MPa | 2070 psi | ASTM D638 |
Teknor Apex HFFR 2005 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable JacketingAgency Ratings: IEC Unsp.. |
|||
Tensile Strength at Break | 14.3 MPa | 2080 psi | ASTM D638 |
Teknor Apex APEX® 1011 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 14.3 MPa | 2070 psi | 20 in/min at 23°F; ASTM D412 |
Teknor Apex Telcar® TL-1477B AUTO UV BLACK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Strength at Break | 14.3 MPa | 2070 psi | ASTM D638 |
3M Scotchkote™ 165HB Urethane Coating 3M Scotchkote Urethane Coating 165HB is a two component 100% solids urethane coating used for the internal and external protection of steel and concrete pipes, tanks, and vessels. It can be used in .. |
|||
Tensile Strength at Break | 14.3 MPa | 2080 psi | ASTM D412 |
Teknor Apex APEX® 2570-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |