Polymer Property : Tensile Strength at Break = 130 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 - 130 MPa
17400 - 18900 psi
ASTM D683
Loxim 140 01V0 Polycarbonate, 40% Glass Filled, Flame Retardant
Information provided by Loxim Industries
Tensile Strength at Break 100 - 130 MPa
14500 - 18900 psi
ISO 527
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,..