Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.78 MPa @Time 7200 sec |
1998 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7195-1000 TPE Product Description: StarFlex P 7195-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tensile Strength at Break | 13.78 MPa | 1998 psi | AVG; ASTM D412 Method A |
Seals Eastern 4503 Natural Rubber General purpose Natural RubberInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 13.78 MPa | 1999 psi | ASTM D412 |
DuPont Performance Polymers Kalrez® 9100 Fluoroelastomer DuPont™ Kalrez® 9100 is an amber translucent product targeted specifically for PECVD and HDPCVD processes. It has also exhibited excellent performance in "select" etch processes. Kalrez® 9100 has.. |