Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.62 MPa | 1975 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 510 Perfluoroelastomer Greene Tweed’s Chemraz® 510, a perfluoroelastomer, offers an extremely broad range of chemical resistance with a Shore A hardness value of 90. with a temperature range form -22°F to 446Â.. |