Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.72 MPa | 1120 psi | |
S&E Specialty Polymers TufTech™ 5501124 Vinyl Application: Replacement for TPV/TPR materials for application requiring an excellent compression set properties, Weatherable, Elastomeric, Extrusion Molding Compound. Targeting for GMP PVC 088.Info.. |
|||
Tensile Strength at Break | 7.72 MPa | 1120 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2175 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 7.70 MPa | 1120 psi | |
GrafTech eGRAF® SPREADERSHIELD™ SS500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Tensile Strength at Break | 7.70 MPa | 1120 psi | ASTM D638 |
Solvay Specialty Polymers Polidiemme® G/450 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |
|||
Tensile Strength at Break | 7.72 MPa | 1120 psi | ASTM D412 |
Teknor Apex Monprene® MP-2334-R2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.72 MPa | 1120 psi | |
Shin-Etsu Silicones KE-7022U Temperature Resistant Silicone Elastomer KE7022 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 300 °C(67 ~ +570 °F).Typ.. |
|||
Tensile Strength at Break | 7.70 MPa | 1120 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® WT361 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 7.70 MPa | 1120 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 7.72 MPa | 1120 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tensile Strength at Break | 7.70 MPa | 1120 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX S 55 A.01 TPE-S, Shore A55, translucent TPE-SInformation provided by BARLOG plastics GmbH. |