Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 7.58 MPa | >= 1100 psi | ASTM D412 |
S&E Specialty Polymers GPE2001E-ROHS PVC GPE2001E-ROHS flame retardant polyethylene compound designed for wire and cable applications. GPE2001E-ROHS complies with RoHS requirements. GPE2001E-ROHS is suitable for 75°C continuous use and 10.. |
|||
Tensile Strength at Break | 7.60 MPa @Temperature 23.0 °C |
1100 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ D3204-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3204-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Tensile Strength at Break | 7.58 MPa @Temperature 23.0 °C |
1100 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Taiwan PU Corporation UR90 Polyester Urethane Rubber UR90 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1843L1 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1875 Thermoplastic Elastomer Notes: Water; Clear; Adhesion to Polycarbonate Features: High Coefficient of FrictionInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1644L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1881B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1504 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt Strength Uses: Safety ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2432F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2770L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | 20"/min Type 1; ASTM D412 |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-1336G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1875HF Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2770 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |