Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.24 MPa | 1050 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R108BM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R1212A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | |
Shin-Etsu Silicones KE-2090-20A/B Self-adhesive LIMS Silicone ShinEtsu KE209020 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity .. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | |
Shin-Etsu Silicones SFX-14036AU Fluorosilicone Elastomer Product Description Shincor SFX14036AU is normal 75 Durometer fluorosilicone compounds. It is designed to process well in molding applications. Product Features: Excellent fuel and solvent resistanc.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Teknor Apex Monprene® MP 1181 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Teknor Apex Monprene® MP-2320 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Teknor Apex Telcar® TL-2363A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Teknor Apex Telcar® TL-2563A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Compuestos Dominicanos Polycom CH-550055-01 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Compuestos Dominicanos Polycom ME-333660 PVC Compound Applications: Seals for caps Appearance: Clear pelletsInformation provided by Compuestos Dominicanos |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D3759 |
3M Scotch® 5912 Cellophane Tape Scotch® Tape 5972 is a transparent cellophane tape designed for light-duty packaging applications. It is typically used for bag closing, temporary holding, and L-clip applications that do not put s.. |
|||
Tensile Strength at Break | >= 7.24 MPa | >= 1050 psi | |
3M Scotchcal™ 8171 Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Tensile Strength at Break | >= 7.24 MPa | >= 1050 psi | |
3M Scotchcal™ 8174 Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Tensile Strength at Break | >= 7.24 MPa | >= 1050 psi | |
3M Scotchcal™ 8674 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Tensile Strength at Break | >= 7.24 MPa | >= 1050 psi | |
3M Scotchcal™ IJ8171 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Tensile Strength at Break | >= 7.24 MPa | >= 1050 psi | |
3M Scotchcal™ 8671 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Tensile Strength at Break | 7.24 MPa | 1050 psi | ASTM D412 |
Compuestos Dominicanos Polycom CO-160355 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |