Polymer Property : Tensile Strength at Break = 1030 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1030 MPa
150000 psi
Performance Alloys MoldStar® 90 Copper Mold Alloy
Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t..
Tensile Strength at Break 1030 MPa
150000 psi
Stress relieved
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std
All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ..
Tensile Strength at Break 1030 MPa
150000 psi
Hard
Hoskins Manufacturing Chromel® Thermocouple Wire
Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu..
Tensile Strength at Break 1030 MPa
150000 psi
Annealed
California Fine Wire Alloy 436 Platinum/Tungsten Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1030 MPa
150000 psi
Hard
California Fine Wire Alloy 52 Nickel Iron Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1030 MPa
150000 psi
Hard
California Fine Wire Manganin 230 (Shunt) Copper, Manganese, and Nickel Resistance Wire
All values may vary dependent on specific design and usageNickel content modifiedCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1030 MPa
150000 psi
Hard
California Fine Wire Manganin 290 Copper, Manganese, and Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1030 MPa
150000 psi
Hard
California Fine Wire Nickel Alloy 120 Nickel Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 1030 MPa
150000 psi
Hard
California Fine Wire NIFE 5200 Nickel Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.