Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.26 MPa | 1488 psi | Change in tensile strength in air after 3600 hours at 268°F; ASTM D573 |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Tensile Strength at Break | 10.26 MPa | 1488 psi | Air at 212°F, 1008 hr; ASTM D573 |
ExxonMobil Santoprene® 121-80M300 Thermoplastic Elastomer
(discontinued **) A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good.. |