Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.48 MPa @Temperature 60.0 °C |
215 psi @Temperature 140 °F |
JRF-14 days |
3M AC-236 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Tensile Strength at Break | 1.48 MPa @Temperature 60.0 °C |
215 psi @Temperature 140 °F |
JRF-14 days |
3M AC-236 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Tensile Strength at Break | 1.48 MPa | 215 psi | JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C; AMS3276 |
3M AC-275 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Tensile Strength at Break | 1.48 MPa | 215 psi | JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C; AMS3276 |
3M AC-275 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Tensile Strength at Break | 1.48 MPa | 215 psi | JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C; AMS3276 |
3M AC-275 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Tensile Strength at Break | 1.48 MPa | 215 psi | |
3M Weatherban™ 606NF Acrylic Sealant 3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M.. |
|||
Tensile Strength at Break | 1.48 MPa @Temperature 60.0 °C |
215 psi @Temperature 140 °F |
JRF-14 days |
3M AC-236 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |