Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.10 MPa | 160 psi | 7 days in BMS-3-11 ty IV |
3M AC-360 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding.. |
|||
Tensile Strength at Break | 1.10 MPa | 160 psi | 7 days in BMS-3-11 ty IV |
3M AC-360 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding.. |
|||
Tensile Strength at Break | 1.10 MPa | 160 psi | |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |