Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.690 MPa | 100 psi | ASTM D3574 |
3M 4508 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Tensile Strength at Break | 0.690 MPa | 100 psi | T-Block on Aluminum; ASTM D987 |
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Tensile Strength at Break | 0.690 MPa | 100 psi | T-Block on Aluminum; ASTM D987 |
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Tensile Strength at Break | 0.690 MPa | 100 psi | T-Block on Aluminum; ASTM D987 |
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Tensile Strength at Break | 0.690 MPa | 100 psi | Die "A"; ASTM D3759 |
3M 4508 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |