Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 0.0483 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.0483 MPa
7.00 psi
Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density
AboSeal 8104-17 is 80% solids and acrylic-latex based. It comes as one package and in most colors. It is known for its high density. It is the same as 8104-16 for low-odor, adhesion, quick drying an..