Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12 LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr.. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4702-8 Polycarbonate EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi.. |
|||
Izod Impact, Unnotched | 4.86 J/cm @Temperature 23.0 °C |
9.10 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12 LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.86 J/cm | 9.10 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |