Polymer Property : Izod Impact, Unnotched = 8.83 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.83 J/cm
16.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
Izod Impact, Unnotched 8.83 J/cm
16.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
Izod Impact, Unnotched 8.83 J/cm

@Thickness 3.17 mm
16.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Izod Impact, Unnotched 8.83 J/cm

@Thickness 3.17 mm
16.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Trirex® 3025A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Izod Impact, Unnotched 8.83 J/cm
16.5 ft-lb/in
ASTM D4812
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled  (discontinued **)
LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat..