Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.67 J/cm
8.75 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC
LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant.
Izod Impact, Unnotched 4.67 J/cm
8.75 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific)
LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br..
Izod Impact, Unnotched 4.67 J/cm
8.75 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI
LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive.