Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.42 J/cm | 8.28 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |