Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 8.19 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP AL004 ABS (Asia Pacific)
LNP* Lubricomp* AL004 is a compound based on Acrylonitrile Butadiene Styrene resin containing Lubricants. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP AL004 ABS
LNP* Lubricomp* AL004 is a compound based on Acrylonitrile Butadiene Styrene resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT
LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON WE002 PBT (Asia Pacific)
LNP STAT-KON* WE002 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF003H PA 66
LNP* THERMOCOMP* RF003H is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF003XXH PA 66
LNP* THERMOCOMP* RF003XXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC
LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched 4.37 J/cm
8.19 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Copyright © lookpolymers.com All Rights Reserved