Polymer Property : Izod Impact, Unnotched = 8.16 J/cm
Polymer Property :
Izod Impact, Unnotched =
8.16 J/cm
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Unnotched
8.16
J/cm
15.3
ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal
LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass.