Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.00 - 5.07 J/cm | 7.50 - 9.50 ft-lb/in | Average value: 4.36 J/cm Grade Count:3 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GM30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech CamAlloy /ABS Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech Korad® SP-9011 Cap ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Spartech SP-9010 General Purpose ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.17 mm |
7.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® ABS/PBT GF15 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |