Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Izod Impact, Unnotched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Izod Impact, Unnotched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |