Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.23 J/cm | 13.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 7.23 J/cm @Temperature 23.0 °C |
13.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp LL003E PEEK LNP* Lubricomp* LL003E is a compound based on Polyetheretherketone (PEEK) containing PTFE. Characteristics of this grade are: Easy Molding and Internally Lubricated.This data was supplied by SABIC.. |
|||
Izod Impact, Unnotched | 7.23 J/cm | 13.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |