Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.09 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
Izod Impact, Unnotched | 7.09 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 7.09 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |