Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.58 J/cm | 6.70 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® T-10 10% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |