Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.57 J/cm | 6.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Izod Impact, Unnotched | 3.57 J/cm | 6.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Izod Impact, Unnotched | 3.57 J/cm | 6.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant. |
|||
Izod Impact, Unnotched | 3.57 J/cm | 6.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC (Asia Pacific) LNP* Stat-kon* DEL339XF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant,.. |