Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Izod Impact, Unnotched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Izod Impact, Unnotched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Izod Impact, Unnotched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Izod Impact, Unnotched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber. |
|||
Izod Impact, Unnotched | 6.20 J/cm @Temperature 23.0 °C |
11.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |