Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 27.0 J/cm | 50.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 27.0 J/cm | 50.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS7R PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 27.0 J/cm | 50.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS7R PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 27.0 J/cm | 50.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 27.0 J/cm | 50.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 27.0 J/cm | 50.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |