Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.98 J/cm | 11.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.98 J/cm | 11.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXQ PEI LNP* THERMOCOMP* EC004XXQ is a compound based on Polyetherimide containing 20% Carbon Fiber. |
|||
Izod Impact, Unnotched | 5.98 J/cm | 11.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched | 5.98 J/cm | 11.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific) LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber. |