Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.95 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON JX89626 PES LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |