Izod Impact, Unnotched 5.83 J/cm
10.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.