Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.75 J/cm

@Temperature -30.0 °C
5.15 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Izod Impact, Unnotched 2.75 J/cm

@Thickness 3.20 mm
5.15 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 246 Toughened Polystyrene
Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu..
Izod Impact, Unnotched 2.75 J/cm

@Thickness 3.20 mm
5.15 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 256 Toughened Polystyrene
Characteristics Superior flexibility Good ball drop strength Excellent clarity Easy flow Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric ..
Izod Impact, Unnotched 2.75 J/cm

@Thickness 3.20 mm
5.15 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP EXP 31 Toughened Polystyrene
Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form..