Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 21.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
39.3 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded, Partial Break; ASTM D256 |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature -30.0 °C |
39.3 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1110R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Unnotched | 21.0 J/cm @Temperature 23.0 °C |
39.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HFD4471 PC Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Unnotched | 21.0 J/cm | 39.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |