Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.79 - 10.7 J/cm
7.10 - 20.0 ft-lb/in
Average value: 7.37 J/cm Grade Count:10
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched 3.79 J/cm

@Temperature 23.0 °C
7.10 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied..
Izod Impact, Unnotched 3.79 J/cm

@Temperature 23.0 °C
7.10 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 (Asia Pacific)
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied..
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66
LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific)
LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 3.79 J/cm

@Temperature 23.0 °C
7.10 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp GF008 PSU
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 3.79 J/cm

@Temperature 23.0 °C
7.10 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific)
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 3.79 J/cm

@Temperature 23.0 °C
7.10 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East)
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 119 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant..
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific)
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON MFD02 PP
LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.79 J/cm
7.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific)
LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.