Polymer Property : Izod Impact, Unnotched = 3.68 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.68 J/cm
6.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66
LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing 20% Aramid. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 3.68 J/cm
6.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 (Asia Pacific)
LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing Aramid. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4702-15 Polycarbonate
EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res..
Izod Impact, Unnotched 3.68 J/cm
6.89 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP MX89510 PP
LNP* THERMOCOMP* MX89510 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.68 J/cm
6.89 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 415 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.