Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.48 J/cm
6.52 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP
LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
Izod Impact, Unnotched 3.48 J/cm
6.52 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Izod Impact, Unnotched 3.48 J/cm
6.52 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 3.48 J/cm
6.52 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific)
LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.
Izod Impact, Unnotched 3.48 J/cm
6.52 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific)
LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..