Mechanical Properties Metric English Comments
Izod Impact, Unnotched 14.4 J/cm

@Thickness 3.17 mm
27.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF40 A1 BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: Lubricated, Low Shrinkage and Good Wear ResistanceAppearan..