Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 25.2 J/cm @Temperature 23.0 °C |
47.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Colorcomp DX98735 PC LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 25.2 J/cm | 47.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP COLORCOMP DX98735H PC LNP* COLORCOMP* DX98735H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare. |