Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 12.17 J/cm
22.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP FARADEX DX11003 PC (Europe-Africa-Middle East)
LNP FARADEX DX11003 is a compound based on Polycarbonate resin potentially suitable to meet high frequency electromagnetic absorption requirments. The compound is also an excellent candidate for man..
Izod Impact, Unnotched 12.17 J/cm
22.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DD000 PC
LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched 12.17 J/cm
22.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific)
LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 12.17 J/cm
22.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.