Polymer Property : Izod Impact, Unnotched = 20.6 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
PolyOne LubriOne™ NN-000/10T-2S Black Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 ..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF006XXY PA 66
LNP* Thermocomp* RF006XXY is a compound based on Nylon 66 containing 30% Glass Fiber.
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP 9X11427
LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G..