Polymer Property : Izod Impact, Unnotched = 2.70 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
5.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D4812
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Unnotched 2.70 J/cm

@Temperature 23.0 °C
5.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS)
Information provided by PolyOne
Izod Impact, Unnotched 2.70 - 5.23 J/cm
5.06 - 9.80 ft-lb/in
Average value: 3.71 J/cm Grade Count:3
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev..
Izod Impact, Unnotched >= 2.70 J/cm
>= 5.06 ft-lb/in
ASTM D256
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE
Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®.
Izod Impact, Unnotched >= 2.70 J/cm
>= 5.06 ft-lb/in
ASTM D256
Forever Plast Namtene® Recycled Standard HDPE
Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications.
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT
LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral
Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss...
Izod Impact, Unnotched 2.70 J/cm

@Thickness 3.18 mm
5.06 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
Izod Impact, Unnotched 2.70 J/cm

@Thickness 3.18 mm
5.06 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S..
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit..
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON LX00797C PEEK
LNP* STAT-KON* LX00797C is a compound based on Polyetheretherketone containing Proprietary Filler(s). Added features of this material include: ristics of this grade are: Clean Compounding System, ..