Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal (Asia Pacific) LNP STAT-KON* KEP33 is a compound based on Acetal resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 273 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |