Polymer Property : Izod Impact, Unnotched = 2.00 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class ..
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade
Data provided by North Wood Plastics, Inc.
Izod Impact, Unnotched 2.00 J/cm

@Thickness 3.20 mm
3.75 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 243 Toughened Polystyrene
CharacteristicsGood flexibility Good clarity High stiffnessProcessing Extrusion ThermoformingApplications Clear thermoformed containers Oriented PS films LidsMaterial Status: Commercial : ActiveA..
Izod Impact, Unnotched 2.00 J/cm

@Thickness 3.20 mm
3.75 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 253 Toughened Polystyrene
Characteristics High rigidity Improved toughness Good clarityProcessing Injection moldingApplications Ball pens Small appliances housings Small impellersMaterial Status: Commercial : ActiveAgenc..
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
Notch Status Unknown
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved