Polymer Property : Izod Impact, Unnotched = 18.7 J/cm - NB Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 18.7 J/cm - NB
35.0 ft-lb/in - NB
Average value: 18.7 J/cm Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 18.7 J/cm
35.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC
LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated.