Polymer Property : Izod Impact, Unnotched = 17.3 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 9.23 J/cm
17.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC
LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 9.24 J/cm
17.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46
LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized.
Izod Impact, Unnotched 9.23 J/cm
17.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC
LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 9.23 J/cm
17.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Izod Impact, Unnotched 9.23 J/cm

@Temperature 23.0 °C
17.3 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 9.23 J/cm
17.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.