Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.80 - 9.20 J/cm @Temperature 23.0 °C |
16.5 - 17.2 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 214 Rigid PVC, Antishock Extrusion Antishock rolling shutters |
|||
Izod Impact, Unnotched | 8.80 - 9.20 J/cm @Temperature 23.0 °C |
16.5 - 17.2 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 704 Rigid PVC, Antishock Extrusion Antishock spiral pipes |
|||
Izod Impact, Unnotched | 8.80 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
Izod Impact, Unnotched | 8.80 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 8.80 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Izod Impact, Unnotched | 8.80 J/cm @Temperature -30.0 °C |
16.5 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Izod Impact, Unnotched | 8.81 J/cm @Temperature 23.0 °C |
16.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Izod Impact, Unnotched | 8.83 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
Izod Impact, Unnotched | 8.83 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
Izod Impact, Unnotched | 8.83 J/cm @Thickness 3.17 mm |
16.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 8.83 J/cm @Thickness 3.17 mm |
16.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.80 - 9.20 J/cm @Temperature 23.0 °C |
16.5 - 17.2 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ARC 30 Rigid PVC, Atoxic for General Purpose Bottles very high antishock |
|||
Izod Impact, Unnotched | 8.83 J/cm | 16.5 ft-lb/in | ASTM D4812 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |