Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Izod Impact, Unnotched | 8.18 J/cm | 15.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC LNP THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 8.18 J/cm | 15.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC (Asia Pacific) LNP* THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 8.16 J/cm | 15.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |